ARON CERAMIC High-Temperature-Resistant Adhesive
ARON CERAMIC is a versatile, one-part heat-curing inorganic adhesive, filler, and coating developed by Toagosei Chemical Industry of Japan after many years of research. It contains no organic matter and is based mainly on refractory ceramics such as alumina and inorganic polymers. It withstands bonding temperatures up to 1,200°C and offers high-temperature resistance, nonflammability, excellent solvent resistance, low toxicity, and high tensile strength.
Properties
· After heat treatment at 150°C, it withstands temperatures up to 1,100–1,200°C without generating gas.
· Provides high bonding strength to metals, ceramics, glass, quartz, carbon, and other materials, even at high temperatures.
· Excellent resistance to thermal cycling.
· Excellent resistance to oil, solvents, chemicals, and moisture.
· In addition to bonding, it can be used for filling, sealing, and coating.
Applications
· Filling gaps around heating elements.
· Heat-resistant bonding of metals, ceramics, glass, quartz, carbon, and other materials.
· Suitable where resistance to solvents, oils, chemicals, and gases such as trichloroethylene, kerosene, and ozone is required.
· Heat-resistant, oxidation-resistant, and wear-resistant coatings for metals and other materials.
· Can be used as a heat-resistant molding material.
· Filling and bonding of explosion-proof equipment and electrical control devices.
· Securing halogen-lamp bases.
· Assembly with spark plugs.
Directions for Use
· For best results, remove rust, oil, and other contaminants from the adherend surface and clean it thoroughly.
· This product is strongly alkaline. Wear gloves during use. If contact occurs, rinse immediately with clean water.
· This product contains a paste body and aqueous solvent and will settle during prolonged storage. Its viscosity can be adjusted to suit the process: use the paste directly for higher viscosity or mix in a small amount of the aqueous solvent to reduce viscosity. It is highly convenient to use.
Bonding
· Apply ARON CERAMIC evenly to the adherend, join the parts, and leave at room temperature for at least 16 hours.
· Dehydration: Heat in an oven at 90°C for 1–2 hours.
· Then heat at 150°C for one hour.
· Remove and allow to cool naturally at room temperature.
Filling
· Inject ARON CERAMIC into the area to be filled and leave at room temperature for at least 24 hours.
· Dehydration: Heat in an oven at 90°C for 1–2 hours.
· Then heat at 150°C for one hour.
· Remove and allow to cool naturally at room temperature.
Coating
· Apply ARON CERAMIC evenly to the object and leave at room temperature for at least 24 hours.
· Dehydration: Heat in an oven at 90°C for 1–2 hours.
· Then heat at 150°C for one hour.

Grades
| Test Item | C-TYPE | D-TYPE | E-TYPE | W-TYPE | |
|---|---|---|---|---|---|
| Before Curing | Appearance | White One-Part Paste | White One-Part Paste | White One-Part Paste | White One-Part Paste |
| Viscosity (cP/25°C) | 70,000 | 50,000 | 50,000 | 50,000 | |
| Density (g/cm3) | 1.9 | 2.3 | 2.3 | 2.3 | |
| Main Component | Silica | Alumina | Silica | Alumina | |
| pH | 12 | 12 | 12 | 12 | |
| Curing Method | Refer to the instructions above. | ||||
| After Curing | Bond Strength (kgf/cm2) | 200 | 250 | 200 | 200 |
| Heat-Resistance Temperature (°C) | 1,200 | 1,300 | 1,300 | 1,300 | |
| Coefficient of Linear Expansion (/°C) | 13 × 10-6 | 8 × 10-6 | 4 × 10-6 | 8 × 10-6 | |
| Thermal Conductivity (kcal/m·hr·°C) | 0.57 | 0.68 | — | 0.68 | |
| Compressive Strength (kgf/cm2) | 1,600 | 2,000 | 1,900 | 1,600 | |
| Flexural Strength (kgf/cm2) | 450 | 600 | 600 | 600 | |
| Vickers Hardness (HV20) | 260 | 420 | 380 | 400 | |
| Volume Resistivity (Ω·cm) | 6 × 109 | 8 × 1010 | 1 × 1010 | 8 × 1010 | |
| Surface Resistivity (Ω) | 3 × 108 | 7 × 108 | 4 × 108 | 7 × 108 | |
| Dielectric Strength (V/mm) | 2,800 | 4,200 | 2,800 | 4,200 | |
| Moisture Absorption (%) | 4 | 2 | 2 | 0.4 | |
| Water Resistance | Good | Good | Good | Excellent | |
| Acid Resistance | Excellent | Excellent | Good | Excellent | |
| Alkali Resistance | Good | Excellent | Good | Good | |
| Oil Resistance | Excellent | Excellent | Excellent | Excellent | |
| Organic-Solvent Resistance | Excellent | Excellent | Excellent | Excellent | |
| Features |
High Bond Strength High Coefficient of Linear Expansion |
High Bond Strength Medium Coefficient of Linear Expansion Good Mechanical Properties |
High Bond Strength Low Coefficient of Linear Expansion Good Thermal-Shock Resistance |
High Bond Strength Water and Moisture Resistance | |
| Primary Application | Primarily for Bonding and Filling Metals | Bonding, Filling, and Coating Materials with Medium Thermal Expansion | Bonding, Filling, and Coating Materials with Low Thermal Expansion | Bonding, Filling, and Coating Materials Requiring Water and Moisture Resistance | |